Tin Cans technical process requirements
1. Cutting material
1)Iron material must be qualified material after inspection
2)Trial cutting before cutting material to do the first piece, the first piece qualified before cutting large material
3)The vertical deviation of the material is ≤0.2mm
4)No indentation, scratching is allowed under the material
(5) cutting material edge can not have phi
2.Angle cutting
1)According to the size of Iron Box box body roll line, determine the appropriate corner cutting size and shape
(2) Neat cut, consistent size, no burrs, no scratches.
3. Line up
(1) The degree of thread starting matches with the diameter of the rolled thread
(2) No scratches and deformation in the process of thread starting
4.Bumping
The embossing position is accurate, with an allowable deviation of 0.2mm or less; the depth of embossing is suitable, and the standard is clear outline and good effect of embossing under normal circumstances without serious distortion and deformation, with a concave depth of 0.4±0.1mm for flat embossing and a strong sense of three-dimensionality and beauty for embossing.
5. Forming
Forming structure, size and size of the drawings match, surface scratching according to the standard judgment, can not have the phenomenon of disguise
6.Buckle bone
The combination of buckle joint is even and smooth. Can not have significant wrong angle, scraping, piercing iron, loose bone phenomenon
7.Buckle bottom
Bottom and Tinplate The lower part of the box body rolled line fastening closely, tight pressure does not loosen, do not fall off.
8. Rolling line
Evenly rolled line, smooth, in place, the line size meets the requirements, and the cover or inner cover with the appropriate degree of elasticity
9. Turning edge, playing tendons, rolling tendons
Size position meets the requirements, uniform size and consistency, visual tendon position neatly, no collapse, scraping, steep edge phenomenon, tendon line uniform smooth and beautiful
10. Bottom sealing
Visual inspection of the periphery can not have dog teeth and unevenness, can not have incomplete rolled edge, double lines, scratching and other undesirable phenomena, the seal bottom is tight, beautiful lines.
11. Stamping
1)Adjust the stamping position first to ensure that it is in line with the drawing.
2)Prevent surface dragging when taking strip material
3)Stamping stretching depth is in accordance with product size requirements
4) The shape and size of the stamping should be in line with the standard after forming.
5)Prevent scratching and deformation in stamping process
If you are interested in the product, contact 2bvideo.com for more information for more information
The information of 2bvideo.com limited shown above is provided by the user or collected on the network. Video 2B does not guarantee the authenticity,accuracy and legitimacy of 2bvideo.com limited information. Video 2B does not involve legal relationships and disputes between users arising from transactions other than secured transactions on this website. Disputes shall be settled by you through negotiation. If you are the person in charge or relevant employee of this enterprise, if you find that the enterprise information is incorrect or want to manage thiscompany, please contact us jacklee1558@gmail.com, after you claim the enterprise, you can obtain management permission, publish supplyand demand information, bring consulting orders, and remove page advertisements.
Main Product:
Tin Box,
Metal Box ,
Metal Can,
Metal Packaging,
Iron Box,
Packaging Can